HASS Mortar
HASS thin-bed mortar is a one-component dry-mix mortar that is ready to use after mixing with water. It is workable, has high bonding strength, does not shrink and reduces waste during installation.
View technical specifications ↓
Mortar, plaster & skimcoat
HASS Mortar
A complete finishing system for HASS AAC blocks and ALC panels: thin-bed mortar, plaster and skimcoat — ready to use after mixing with water.
Three materials
Products
HASS Mortar
HASS thin-bed mortar is a one-component dry-mix mortar that is ready to use after mixing with water. It is workable, has high bonding strength, does not shrink and reduces waste during installation.
View technical specifications ↓
HASS Plaster
HASS Plaster is a one-component dry-mix plaster ready to use after mixing with water, helping reduce material loss during application.
View technical specifications ↓
HASS Skimcoat
HASS Skimcoat is a thin finishing coat for HASS AAC blocks and ALC wall panels. It creates a smooth surface before painting, protects the wall and improves paint durability.
View technical specifications ↓
Data
Technical specifications
Factory test results excerpted from the quality certificate issued with each batch. Select a product to view its table. For the full batch certificate, call 0931 532 456.
Applicable standard: TCVN 9028:2011 · Color: grey · Packing: 50 kg bag
| No. | Quality criterion | Unit | Requirement | Test result |
|---|---|---|---|---|
| 1 | Maximum aggregate particle size | mm | ≤ 1.25 | 1.2 |
| 2 | Flow value | mm | 180 ~ 210 | 195 |
| 3 | Flow retention | % | ≥ 90 | 95 |
| 4 | Initial setting time | min | ≥ 180 | 200 |
| 5 | Adjustment time | min | — | 6 |
| 6 | Capillary water absorption coefficient | kg/m² | ≤ 0.2 | 0.1 |
| 7 | Chloride ion content in mortar | % | ≤ 0.1 | 0.023 |
| 8 | Average compressive strength | MPa | ≥ 7.5 | 12 |
| 9 | Bond strength | MPa | ≥ 0.4 | 0.7 |
Applicable standard: TCVN 9028:2011 · Color: grey · Packing: 50 kg bag
| No. | Quality criterion | Unit | Requirement | Test result |
|---|---|---|---|---|
| 1 | Maximum aggregate particle size | mm | ≤ 1.25 | 1.2 |
| 2 | Flow value | mm | 180 ~ 210 | 190 |
| 3 | Flow retention | % | ≥ 90 | 92 |
| 4 | Initial setting time | min | ≥ 180 | 200 |
| 5 | Adjustment time | min | — | — |
| 6 | Capillary water absorption coefficient | kg/m² | ≤ 0.2 | 0.1 |
| 7 | Chloride ion content in mortar | % | ≤ 0.1 | 0.023 |
| 8 | Average compressive strength | MPa | ≥ 7.5 | 14 |
| 9 | Bond strength | MPa | ≥ 0.4 | 0.8 |
Applicable standard: TCVN 7239:2014 · Color: grey · Packing: 50 kg bag
| No. | Quality criterion | Unit | Test result |
|---|---|---|---|
| 1 | Maximum aggregate particle size | mm | < 0.7 |
| 2 | Flow value | mm | 180 – 210 |
| 3 | Flow retention | % | > 90 |
| 4 | Initial setting time | min | > 180 |
| 5 | Chloride ion content in mortar | % | < 0.1 |
| 6 | Average compressive strength | MPa | > 2.5 |
| 7 | Bond strength | MPa | > 0.2 |
| 8 | Capillary water absorption coefficient | kg/m²·min⁰·⁵ | 0.1 |
Construction insights and trends
Blog

How to calculate AAC blocks for a house — and 3 mistakes that cause shortages or surplus

Latest HASS AAC block and ALC panel price guide 2025 — economical, durable and modern building materials

Fast and safe construction with AAC blocks

Lightweight construction material trends in 2025

Heat reduction for west and southwest-facing homes — a multi-layer, energy-efficient solution

House fire risks and effective fire-resistant solutions with HASS AAC

View all articles ››
Other products